Hi, can we use  POP as mold material for CFRP prepreg component??
maximum temperature for curing-120 degree

Reply
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh no, my experience is very much in line with yours. Tool sealers do a good job, but I haven't ever managed to get anything close to the surface finish I can get with traditional mould making. For me the only way to do it is to make splash moulds and then new patterns that can be polished to a higher standard and then remake the final moulds. Its tedious and not an ideal way to do things, especially if accuracy is critically important. Making copies of copies always results in some degree of dimensional change.

This is really why I dont use much epoxy tooling board. When I mill things, I mill it from polyurethane tooling board and pattern coat them (the thickness of which is taken into account when doing the CAD model), then make moulds the old fashioned way.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Gaurav Kumar Thakur - 6 Years Ago
Hanaldo - 6 Years Ago
Gaurav Kumar Thakur - 6 Years Ago
torstenker - 6 Years Ago
Hanaldo - 6 Years Ago
Gaurav Kumar Thakur - 6 Years Ago
torstenker - 6 Years Ago
Hanaldo - 6 Years Ago
Rosta Spicl - 6 Years Ago
Hanaldo - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search