How do I put carbon over a block of foam?


Author
Message
torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
I would suggest to cut is insitio, when putting it on, this was you can press the fabric into the base coat preventing the end from comming out


torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
I would cut the fibre while pressing it onto the base coat,the image was only a demo how to overlap
you can do multiple sections, does not have to be one piece, that may be better because you cube is quiet small

torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
how did you get on with the cube
Fastskiguy
F
Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)
Group: Forum Members
Posts: 11, Visits: 18
torsten Ker - 10/23/2020 11:53:21 AM
how did you get on with the cube

Not good (yet).

I picked up some cheap fiberglass and it is more flexible and cheaper while I try to figure out how to do this. It's those damn corners. I need a cube with fewer corners I think Wink

Getting it all tacky then sticking it on with my hands is working pretty well. I'm using masking tape to hold the edges then after it hardens I can peel the tape off. Doing one edge at a time and simply overlapping the fabric wherever it happens to land. Once I get a cube actually covered with fabric and epoxy I am hoping I can fine tune my procedure. 

I'm really surprised I'm struggling so much. Back in the 80's I made a surfboard and I don't remember having any kind of trouble like this!

Joe

torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
if you make 3 carbon pieces,
1 long one to cover the shorter sides with one long 1" wide strip in one go with opverlapping the corners and and then later cover the top and bottom 6"x3 1/2" sides
sometimes I use cling film to hold the overlapping corners down by wrapping it on top of the fibre

and you need a very sticky basecoat like the XRC basecoat, may get a small quantity on EC's website


Edited 6 Years Ago by torsten Ker
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
A cube is significantly harder to wrap than a surfboard. All about the radius! 

I would actually suggest not trying to wrap around the corners, but rather try the technique demonstrated in EC's skinning tutorial (skip to 6:25):

https://youtu.be/aqwhcfQZT8U

To do that, I would cut 6 individual pieces of carbon that are each slightly larger than the sides of the cube, and stick them down to the base coat. When the base coat has hardened more, trim off most of the excess but leave a 2 or 3mm overhang as Paul demonstrates in the video, wet the carbon out with resin, and then once hardened you can sand the carbon back to the shape of the cube. That will give you a very nice neat seam on all of the radius that will be quite hard to spot, but avoid the problems you are having.
Fastskiguy
F
Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)
Group: Forum Members
Posts: 11, Visits: 18
I like both of those ideas....I'm going to try both of them! Thanks guys Smile
Fastskiguy
F
Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)
Group: Forum Members
Posts: 11, Visits: 18
Fastskiguy - 10/23/2020 11:54:18 PM
I like both of those ideas....I'm going to try both of them! Thanks guys Smile

The 6 piece experiment went pretty well but the 3 piece went even better....one large to go around and two small pieces on the ends. Now....do I just grab a sanding block and go to town on those edges?


Attachments
6 piece.jpg (311 views, 2.00 MB)
3 piece.jpg (202 views, 2.00 MB)
Fastskiguy
F
Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)Supreme Being (135 reputation)
Group: Forum Members
Posts: 11, Visits: 18
Fastskiguy - 10/27/2020 7:28:44 PM
Fastskiguy - 10/23/2020 11:54:18 PM
I like both of those ideas....I'm going to try both of them! Thanks guys Smile

The 6 piece experiment went pretty well but the 3 piece went even better....one large to go around and two small pieces on the ends. Now....do I just grab a sanding block and go to town on those edges?