Group: Forum Members
Posts: 135,
Visits: 1.6K
|
Also, make sure that your catchpot is indeed leak proof. I performed a drop test over 20 mins and nothing changed on my bag, so I infused. Then I clamped off the lines. Yet I left the catchpot in a vacuum with the pump.
In the morning I came to check, infusion was very good, catchpot had lost about an 1/8th of vacuum.
And the mesh has never punctured my regular bagging film. That is some tough stuff, not that easy to puncture, you feel how strong it is when cutting the holes for inlet/outlet. Shouldnt be a problem.
cheers
|