Hi guys,

I had a few experiments to cast a rubbing strip for oldtimer bumpers (middle of the bumper).  So these cars aren't outside for months, but strip needs to be sort of weather proof


So I bended a aluminium for mould, shape is perfect.

After using some casting rubbers (including UV stabilisator) I keep having strange complications.

UV really kicks in after 14 days:


strange spots after rain:

color fading away after 14 days


is there someone who can point me to the right (easy comp) kind of product?  needs to be a little flexible / soft ...

thanks in advance !!


Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If it is not fully cured, it will still be hydroscopic. 24 hours may be fine for demould but, like most resin systems, the tail end of the resin cure may be longer.  I would leave it a good week to fully cure or do a post cure in an oven before putting outside.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search