By dubster - 10/1/2020 2:18:05 PM
Hi guys,
I had a few experiments to cast a rubbing strip for oldtimer bumpers (middle of the bumper). So these cars aren't outside for months, but strip needs to be sort of weather proof

So I bended a aluminium for mould, shape is perfect.
After using some casting rubbers (including UV stabilisator) I keep having strange complications.
UV really kicks in after 14 days:

strange spots after rain:
 color fading away after 14 days

is there someone who can point me to the right (easy comp) kind of product? needs to be a little flexible / soft ...
thanks in advance !!
|
By dubster - 10/12/2020 6:25:59 AM
UR 3450 Sika
|
|