	Group: Administrators 	        
    Posts: 134, 
    Visits: 614 
    
 
          
		     | 
				                       
                 
                
                    
			            Hi Rob, 
  Normal cutting fluids will not harm the carbon laminate, oils and solvents can be an issue as they can penetrate the edge slightly so avoid these, once the components have been milled you should rinse them is fresh water and then dry them off, you should be fine to go ahead!                
			            
  				
			            Paul Statham Easy Composites / Carbon Mods - Technical                     
                     
                                            
                         
                    
                  
             |