Hi,
what are the scenarios where is better to use a semi permanent release agent and the ones where is better a wax?
Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Lester Populaire - 10/5/2020 5:12:20 AM
Massimiliano - 10/5/2020 3:45:35 AM
Hi,
what are the scenarios where is better to use a semi permanent release agent and the ones where is better a wax?

I use wax for surfaces that have some level of porosity (like body filler) and surfaces that are not resistant to solvents. Usually permanent releases for everything else even tho we started using formula five wax for more and more things to reduce exposure to solvents. 

Thank you

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
             Thank you
mporta71 - 5 Years Ago
Fasta - 5 Years Ago
mporta71 - 5 Years Ago
Fasta - 5 Years Ago
                     Understood, thank you!
mporta71 - 5 Years Ago
Warren (Staff) - 5 Years Ago
             Thank you for the additional advice
mporta71 - 5 Years Ago
chriscnf - 5 Years Ago
Fasta - 5 Years Ago
chriscnf - 5 Years Ago
Fasta - 5 Years Ago
                             Thanks...appreciate you help and this forum...brilliant
chriscnf - 5 Years Ago
carguy84 - 4 Years Ago
Hanaldo - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search