Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
The backing plate will only work if your polisher has the same fixing arrangement. Most professional polishing machines will have the right fixing on it. Some cheaper polishing machines do not.
Your polisher looks the right kind of fixing. The pad has an M14 female thread.