Need help with repair on infiusion part?


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As said above, repair patches on the back will give you strength.  You will need some resin or paint to try and hide the crack on the front. Be it a thin resin coat to hide the crack which is sanded back smooth, or a few coats of lacquer.  Ideally fill the crack in first before going near paints as you may need a few coats to stop it just sinking into the crack.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Classicarbon
C
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 86, Visits: 639
Which of those will be the best for repair. I know that one say it's especially for repairs.But is it only curing time difference between two?

Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If you are in a rush, then the rapid repair is a lot quicker curing and also offers some mechanical advantage in terms of flexural strength under impact and loading. Otherwise the El2 is a good all round laminating epoxy and would still give very good results but with more reasonable pot lives with the 2 hardener options. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search