I get that crak when my part stuck in mould. Can you help how to repair it? Should I make patch underneath to reinforced also? Thanks
|
By Warren (Staff) - 10/5/2020 2:25:12 PM
If you are in a rush, then the rapid repair is a lot quicker curing and also offers some mechanical advantage in terms of flexural strength under impact and loading. Otherwise the El2 is a good all round laminating epoxy and would still give very good results but with more reasonable pot lives with the 2 hardener options.
|
|