I get that crak when my part stuck in mould. Can you help how to repair it?
Should I make patch underneath to reinforced also?
Thanks
Reply
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
torsten Ker - 9/28/2020 12:19:40 PM
thats a 0.5mm thickness, you may be able to carefully send a bit down on the outside so that the outside patch does not stick out too much, patch it.
Don't forget tho drill the end of the crack, once done on the outside re-enforce the inside.

How do you done finish the part, spray paint or XCR coating resin. The latter will get the best result to hide it best as possible
May be faster and cheaper to do a new part

Not afford at the moment ๐Ÿ‘Ž๐Ÿ˜”.need to do the repair. 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Classicarbon - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
torstenker - 5 Years Ago
Classicarbon - 5 Years Ago
torstenker - 5 Years Ago
Classicarbon - 5 Years Ago
torstenker - 5 Years Ago
Classicarbon - 5 Years Ago
explorecomposites - 5 Years Ago
Warren (Staff) - 5 Years Ago
Classicarbon - 5 Years Ago
Warren (Staff) - 5 Years Ago