I would like to try MTI hose. Out of curiosity I took a 2 foot section of MTI hose, added an elbow at one end, sealed it with yellow sealant tape, at the open end I wrapped and sealed it with sealant tape, then applied vacuum. The MTI Hose holds at 20 very well. I thought the white covering was supposed to be porous and let the gasses seep  through while blocking the resin? I’m I supposed to take a fine needle and poke holes through the membrane to get it to work? Thanks, Allen
Replies
Kacordy
K
Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)
Group: Forum Members
Posts: 17, Visits: 341
Hanaldo - 9/23/2020 12:18:24 AM
Kacordy - 9/22/2020 4:35:13 PM
I’m I supposed to take a fine needle and poke holes through the membrane to get it to work? Thanks, Allen

Certainly not!

I'm not sure what youve done wrong here, but something is wrong. Can you post a picture of what you tried?

Have a look on YouTube for MTI Hose, DD-Compound themselves and lots of others have some good videos where you can see how to use the hose correctly.

Check this out. I hooked up vacuum to one end of the MTI hose and plugged the other end. Apply vacuum and the MTI hose is sealed and holds vacuum perfectly. So how is the MTI hose used under the vacuum bag to remove air and draw resin into the mold? Look closely and the white outer liner is wrinkled because the vacuum has drawn the material in. Here is a picture. The white material is not porous. If it was porous it would not hold vacuum. Check out the gauge at 20.  Allen 

Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Kacordy - 9/23/2020 2:45:45 AM
Hanaldo - 9/23/2020 12:18:24 AM
Kacordy - 9/22/2020 4:35:13 PM
I’m I supposed to take a fine needle and poke holes through the membrane to get it to work? Thanks, Allen

Certainly not!

I'm not sure what youve done wrong here, but something is wrong. Can you post a picture of what you tried?

Have a look on YouTube for MTI Hose, DD-Compound themselves and lots of others have some good videos where you can see how to use the hose correctly.

Check this out. I hooked up vacuum to one end of the MTI hose and plugged the other end. Apply vacuum and the MTI hose is sealed and holds vacuum perfectly. So how is the MTI hose used under the vacuum bag to remove air and draw resin into the mold? Look closely and the white outer liner is wrinkled because the vacuum has drawn the material in. Here is a picture. The white material is not porous. If it was porous it would not hold vacuum. Check out the gauge at 20.  Allen 

does it hold this vacuum level when you turn off the pump? there is obviously some restriction with the MTI hose.

I usually pull the initial vacuum through the resin feed side to get all the air out quickly.

cheers

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Kacordy - 9/23/2020 2:45:45 AM

The white material is not porous. If it was porous it would not hold vacuum. Check out the gauge at 20.  Allen 

I can not tell from the photo what you are doing, but you are jumping to conclusions here. I can assure you the white material is a semi-permeable membrane, and it works as intended when used properly. Not only have I used it personally, but it is an award winning internationally used product. DD-Compound post on here semi-regularly, so they will probably be along in a bit and reply themselves.

In the meantime, this is a very strange test. 20mm/Hg is no where near full vacuum, which indicates that you are pulling against a major air leak - likely the MTI hose. It is very difficult to see any wrinkles in the hose in that photo, but to me that looks like the hose when it is not under vacuum. 

Watch this video, this is how you use the hose:


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Kacordy - 5 Years Ago
Hanaldo - 5 Years Ago
Kacordy - 5 Years Ago
SleepingAwake - 5 Years Ago
Hanaldo - 5 Years Ago
Warren (Staff) - 5 Years Ago
Kacordy - 5 Years Ago
DD-Compound - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search