The chemical release agents are the top quality what you can use. There is no need apply others like a PVA or waxes. I'd like recommend don't use anything other if the chemical release agent has been already applied. From my point of view the best to sand and polish all the mould to be sure, all the layers of release agents you used are gone. It seems the mould is black epoxy gelcoated, OK, but the surface has a microscopical porosity, that's the reason to use filler (for example Frekote FMS) for first 2-3 layers before release agent. The 5-6 coats of easylease are obviously enought. Are you absolutely sure, there are no negative draft locks on the mould? Especially around the inner rounded corners.
|