By jeffrey bres - 9/20/2020 7:28:06 AM
hi all.
i recently made my first rc boat mould using the unimould system. i used pva for the bottom part of the plug. and easylease and pva for the top half.
these came out fairly well. but not as smooth finich as i hoped. so hours of wetsanding and buffing later..
i put on 7 layers of easy lease. eg60 transparent gelcoat 2 layers as even as i could with brush. 2x 200 glass 1 carbon (240 or zo i believ) and another 2x 200 glass. for the deck half. in the sharp corners i made a fillit of epoxy and thixotr...between the gelcoat and the glass to have the sharp corners evened out. so far so good. al went in super smooth.
30 hours later. i wanted to pull the part.....
i allmost thought i would break my mould. the edges with the fillit where so stuck!.
now i think i put the release agent on and buffed to hard.
heres question 1. i cleaned the mould. put the easy lease on thicker. didnt buff at all. and i read i can wax it. now before i want anything on top of the easy lease. what do i do when i pull it. do i need to clean it completely and stard over with the easylease. or can i just remove the wax and doe 1 or 2 new coats of easy on it.
|
By jeffrey bres - 9/22/2020 11:21:42 PM
i know. will be in future.
|
|