Post Curing even when 2k clearing?


Author
Message
bennyT
b
Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)
Group: Forum Members
Posts: 11, Visits: 777
Hey All,

I'm just wondering whether the experts on here post cure their carbon fibre parts that are going to be exposed to UV rays even when they are going to 2K clear the part as well.

As I understand it, both methods will protect carbon fibre from UV exposure and stop the item getting soft in the heat so therefore is there a need to do both? 
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Yes that is correct


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
bennyT
b
Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)
Group: Forum Members
Posts: 11, Visits: 777
Warren (Staff) - 9/18/2020 3:24:24 PM
Yes that is correct

Thanks Warren

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search