Group: Forum Members
Posts: 17,
Visits: 341
|
Can I sprinkle 1/4 chopped CF down the center of a complex part to mask the seam of 2 pieces of Kevlar/CF that I will use as a surface veil? I would sprinkle the 1/4 CF to create a 2 inch wide 2 foot long center stripe. Will the infusion epoxy flow through this 2 inch strip? Or will the Chopped CF move. I don’t think it will move because of the layers I will have on top to strengthen the part. I’m talking about doing all this dry, not a wet lay-up. Thanks, Allen
|