Hello,

I need to know either an exact or approximate value for the Poisson's ratio and Young's modulus of a mix of EL2 epoxy laminating resin and AT30 slow epoxy hardener. If you can, could you please help me with that?
Ideally, I would like to know an estimate of what the Poisson's ratio and Young's modulus would be for the following mix:
- 23 g of EL2 epoxy laminating resin
- 7 g of AT30 slow epoxy hardener
- 90 g of sand of size between 0.5 and 1 mm
- 30 g of sand less than 250 micrometer in size

If you cannot help me, do you know of references/papers that could help me?

Cheers!
Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The mechanical data available for EL2 is on the enclosed TDS. However the data is relevant to the resin and not a specific mix of materials and additives.  You would need to try and simulate or calculate data for your specific mix. In practice it may well be easier to mix a test batch and conduct testing on it. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Attachments
EC-TDS-EL2-Epoxy-Laminating-Resin.pdf (1.1K views, 320.00 KB)