Cast car spoiler


Author
Message
johan holm
johan holm
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 6, Visits: 125
Hello
I want to cast a small spoiler for the trunk of my car and thought to do it in polyurethane

Which polyurethane should I cast the final spoiler in? 

I thought I would make the mold in silicone
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You'd have to try it.  These resins have not been tested in automated machines like that.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
johan holm
johan holm
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 6, Visits: 125
Warren (Staff) - 9/11/2020 8:39:26 AM
You'd have to try it.  These resins have not been tested in automated machines like that.

It worked well to make my roof spoiler

Now the next project is 2 small front lips

I thought I would make a 2 piece mold in fiberglass and that the final product would be 3-4 mm thick as the original bumper

Which polyurethane may be suitable? It needs to be more durable than the roof spoiler because it is located in a more exposed place

The Xencast P2 Fast Cast  becomes very hard, is there an alternative that is more flexible but can still be painted?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
johan holm - 6 Years Ago
Warren (Staff) - 6 Years Ago
johan holm - 6 Years Ago
Warren (Staff) - 6 Years Ago
johan holm - 6 Years Ago
Warren (Staff) - 6 Years Ago
johan holm - 6 Years Ago
Warren (Staff) - 6 Years Ago