By johan holm - 9/6/2020 9:58:53 AM
Hello I want to cast a small spoiler for the trunk of my car and thought to do it in polyurethane
Which polyurethane should I cast the final spoiler in?
I thought I would make the mold in silicone
|
By Warren (Staff) - 10/1/2020 11:10:00 AM
Excellent! Glad it worked well.
As an alternative but tougher, you could use the Xencast P6 Toughened Polyurethane Resin but it is a bit more moisture sensitive in mixing and a little bit less user friendly than the P2. You could add milled carbon to the P2 to make it tougher. Both resins can be painted.
|
|