Hello
I want to cast a small spoiler for the trunk of my car and thought to do it in polyurethane

Which polyurethane should I cast the final spoiler in? 

I thought I would make the mold in silicone
Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Depends how thick you want to make it?  Solid PU for anything of any substance, other than a small lip spoiler, would be quite heavy and may need a couple of pours to avoid overheating and shrinkage.

However a typical small lip spoiler, (20mm by 20mm triangle type shape) can be done in any Fast Cast PU such as our Xencast P2 Fast Cast Polyurethane Casting Resin.  I would add some milled carbon fibre for strength then you can paint it once done and bond it into place.

No problem with a silicone mould, just ensure it has a nice support box around it so you know the resulting cast is straight and true relative to the boot lid edge.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
johan holm
johan holm
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 6, Visits: 125
Warren (Staff) - 9/7/2020 4:02:50 PM
Depends how thick you want to make it?  Solid PU for anything of any substance, other than a small lip spoiler, would be quite heavy and may need a couple of pours to avoid overheating and shrinkage.

However a typical small lip spoiler, (20mm by 20mm triangle type shape) can be done in any Fast Cast PU such as our Xencast P2 Fast Cast Polyurethane Casting Resin.  I would add some milled carbon fibre for strength then you can paint it once done and bond it into place.

No problem with a silicone mould, just ensure it has a nice support box around it so you know the resulting cast is straight and true relative to the boot lid edge.

The idea is that it should be hollow without a bottom and 2-3mm thick

Something like this
https://www.amazon.com/06-12-Lexus-IS250-IS350-Spoiler/dp/B00K3YFL66

I plan to make a 2 piece silicone mold with one part as the whole outside then the other part as a bottom and insert with injection holes and some air drainage holes

Is it possible to inject polyurethane with a 2 component pump like this that has a mixing nozzle? 

https://rover.ebay.com/rover/0/0/0?mpre=https%3A%2F%2Fwww.ebay.com%2Fulk%2Fitm%2F163668849571

Best Regards


Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The pot life of most fast cast PU's is going to be too short to use a machine like that. Just ensure your mould has good vent holes and you should be fine.  

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
johan holm
johan holm
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 6, Visits: 125
Warren (Staff) - 9/8/2020 3:55:03 PM
The pot life of most fast cast PU's is going to be too short to use a machine like that. Just ensure your mould has good vent holes and you should be fine.  

The machine I linked to has 2 separate containers one for part A and one for part B and then they are mixed together 50/50 in the nozzle.

Can it work on, for example, Xencast P2 Fast Cast Polyureth

Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You'd have to try it.  These resins have not been tested in automated machines like that.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
johan holm
johan holm
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 6, Visits: 125
Warren (Staff) - 9/11/2020 8:39:26 AM
You'd have to try it.  These resins have not been tested in automated machines like that.

It worked well to make my roof spoiler

Now the next project is 2 small front lips

I thought I would make a 2 piece mold in fiberglass and that the final product would be 3-4 mm thick as the original bumper

Which polyurethane may be suitable? It needs to be more durable than the roof spoiler because it is located in a more exposed place

The Xencast P2 Fast Cast  becomes very hard, is there an alternative that is more flexible but can still be painted?

Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Excellent! Glad it worked well. 

As an alternative but tougher, you could use the Xencast P6 Toughened Polyurethane Resin but it is a bit more moisture sensitive in mixing and a little bit less user friendly than the P2.  You could add milled carbon to the P2 to make it tougher.  Both resins can be painted.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search