Coleagues
Just another issue I´m unsuccesfull.
Trying to laminate a sandwich panel  with nonconstant thickness in 2 steps process. 1st step there is a cca 0.7mm thick panel based on UD carbon prepregs - 1x54+2x100+2x200gsm UD. On 2nd step apply the Rohacell core and inner skin based on twill 200gsm carbon prepreg, see the attchd. sketch. The curing process starts on vac-1bar@100°C for 4.5hours, cooling slow down to 30°C for 6hours. After demoulding the panel is going to distorsion about 10mm.
Any tips for process changes?
Thanks a lot, Rosta


Reply
Chris Rogers
C
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 120, Visits: 933
Looks like you found the problem!  I wouldn't lay all the blame on the unbalanced laminate - tapered core can be an issue too even with balanced skins - but most of it. 

I'm interested in your 54g uni though - what is that and where did you get it?




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search