			            If you get yourself a small block of closed cell foam from EC, you can cut some smaller blocks from this and bond these to the back of the part to give more of a surface on which to bond your signboard flange. 
 The foam can be sanded to the required depth quite easily.
 
 Hot melt glue would work best for bonding and can be pulled away afterwards.
 
 Wax wouldn't work as it wouldn't hold things in place very well. 7
 
 |