Must have tools for carbon fiber


Author
Message
Buchado
B
Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)
Group: Forum Members
Posts: 30, Visits: 208
Hi everyone,

I'm about to graduate in engineering and decided to work with carbon fiber (mainly developing and producing bike parts), so I'm building my work room and would like to know some must have tools/equips to work with carbon fiber.

I have a vaccum pump, a resing catchpot, a degasing chamber, a small mill, a dremel rotary cutter, currently building an oven, but figured I could ask for some advice before building the whole work room, so I can put everything I need in it, willing to work mainly with prepreg and infusion.

So, what are the must have tools to work with carbon fiber?

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It all depends on how much you want to spend.  You want to be looking in our Tools, Equipment & Supplies  section of the website.

You want a decent set of shears to cut the pre-preg.  The snips can be handy too.

The dibber tools and wedges will help with layup and demoulding.

Then a selection from the Perma-Grit section, so cutting disc for your dremel and a selection of tools for sanding and finishing the edges of the parts.

You could also get a wall rack to hold rolls of vacuum bagging consumables.

Obviously don't forget PPE and consumables as these can all add up. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Buchado
B
Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)Supreme Being (421 reputation)
Group: Forum Members
Posts: 30, Visits: 208
Warren (Staff) - 8/14/2020 4:18:23 PM
It all depends on how much you want to spend.  You want to be looking in our Tools, Equipment & Supplies  section of the website.

You want a decent set of shears to cut the pre-preg.  The snips can be handy too.

The dibber tools and wedges will help with layup and demoulding.

Then a selection from the Perma-Grit section, so cutting disc for your dremel and a selection of tools for sanding and finishing the edges of the parts.

You could also get a wall rack to hold rolls of vacuum bagging consumables.

Obviously don't forget PPE and consumables as these can all add up. 

I didn't get a notification for your answer, Warren, thanks for the info.
I live in Brazil, is it possible to buy prepreg from you guys from easy composites?

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Yes we can ship worldwide.  However if it is likely to get stuck in customs, and the temperatures are very hot, then it may use up a lot of outlife. So we recommend ensuring in advance that you are unlikely to have customs issues.  Normally we use an express service to reduce the transit time as much as possible.  Once you get the pre-preg you will need to put it into a freezer again as soon as possible. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ArturK
ArturK
Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)
Group: Forum Members
Posts: 19, Visits: 53
Do not forget about painting - most visual carbon fiber parts need it (UV / humidity- water protection). So spray gun, compressor, and clean room with ventilation for painting .


Carbon fiber sheets and composites .
www.dexcraft.com
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search