I have made some new fuel tank floats out of cork for a vintage vehicle. They need proofing against 100 low lead octane fuel. Can you please recommend a suitable product? In the old days, they were coated with shellac, but having tried and failed I'm now looking for a suitable resin. Thanks.
Replies
Hanaldo
Hanaldo
Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)Supreme Being (14K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Phenol novolac epoxy is the go. 
Dave Reid
D
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 2, Visits: 13
Hanaldo - 8/4/2020 1:35:18 PM
Phenol novolac epoxy is the go. 

Thanks both - I'll give it a try!