Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
General Composites Discussion
Fuel Float
http://www.talkcomposites.com/Topic37619.aspx
By Dave Reid
-
8/4/2020 9:51:43 AM
I have made some new fuel tank floats out of cork for a vintage vehicle. They need proofing against 100 low lead octane fuel. Can you please recommend a suitable product? In the old days, they were coated with shellac, but having tried and failed I'm now looking for a suitable resin. Thanks.
By Dave Reid
-
8/5/2020 5:43:13 AM
+
x
Hanaldo - 8/4/2020 1:35:18 PM
Phenol novolac epoxy is the go.
Thanks both - I'll give it a try!