			            That is unfortunately just the nature of wet laid composites, they are generally full of voids like that and getting consistently good results is very difficult. Won't have anything to do with the release agents used. 
  This is why resin infusion and pre-preg are so highly rated, because it is so much easier to get a consistently void free surface.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |