Styrene mould, release agent


Author
Message
Andy Ricketts
A
Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)
Group: Forum Members
Posts: 4, Visits: 8
Greetings! Newbie here...
I bought the beginners laminating kit which included the PVA release agent. The mould tool was made from Polystyrene with a wooden support, painted with (car) cellulose paint (thoroughly cured). I did wot it said for the release agent, but it didn't release. Sob, sniff. The paint came away in chunks. Wot a mess.....
Any ideas of what I did wrong? Be kind.....
Should I be using the wax release agent? If so, why is there PVA release agent in the kit?
I'm about to start reworking the tool for another go and would prefer to get it right this time!!
For scale, the finished parts are about 150mm amd 100mm long.
TIA

Andy Ricketts