Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Remember the pot life is only relevant to its time in the pot. For a large infusion you use perhaps a kilo at most in the jug at first as it will fly out initially. Then only top it up when it needs it with enough to be used up well within the pot life.
Pot life is dependant on volume of resin, temperature, size of the pot, and other factors.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|