Is this correct?

Roll my mold with GC50 gel coat, wait a few hours till it is tacky but will not adhere to finger, add the reinforcement and infuse with IN2 epoxy.

Thanks...Alan

By ahender - 7/14/2020 4:09:36 PM

Warren (Staff) - 7/14/2020 4:05:31 PM
Remember the pot life is only relevant to its time in the pot.  For a large infusion you use perhaps a kilo at most in the jug at first as it will fly out initially.  Then only top it up when it needs it with enough to be used up well within the pot life.

Pot life is dependant on volume of resin, temperature, size of the pot, and other factors. 