Hi,

I have searched a lot, but I can't find a clear answer to my case.
I am making moulds for the carbon fiber fenders. The moulds are almost ready and I started to wonder if I need to post cure them? They are made from vinylester gelcoat, and polyester resin with fiberglass. If I need to post cure the moulds, how should I do it and do I need to leave the original fender inside the mould while doing it?

And the same applies to curing the parts. I will make the parts from carbon fiber and epoxy using infusion. How those should be cured? Parts inside the moulds or not? I will use this resin: https://composite24.co.uk/infusion-epoxy-resin-1-5kg

Also, how much resin I need? I am guessing that 1.5 kg/fender?


Replies
okkim
o
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 14, Visits: 102
Gelcoat was cured in a room temperature (about 20C). I didn't heat it. So then it must be the paint I used. I'm so pissed right now Sad

I will try to heat it and then maybe add some thinner to break the paint.
okkim
o
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 14, Visits: 102
I got the fenders off! They were super tight!! The paint wasn’t stuck as I thought. I used wooden long wedges to pry those off. First I heated the fenders but it didn’t help.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
okkim - 5 Years Ago
Steve Broad - 5 Years Ago
Warren (Staff) - 5 Years Ago
okkim - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
                     Of course, keep forgetting that we aren't talking prepreg here.
Steve Broad - 5 Years Ago
okkim - 5 Years Ago
Hanaldo - 5 Years Ago
okkim - 5 Years Ago
okkim - 5 Years Ago
oekmont - 5 Years Ago
okkim - 5 Years Ago
Hanaldo - 5 Years Ago
okkim - 5 Years Ago
okkim - 5 Years Ago
Hanaldo - 5 Years Ago
okkim - 5 Years Ago
Warren (Staff) - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search