Hi,

I have searched a lot, but I can't find a clear answer to my case.
I am making moulds for the carbon fiber fenders. The moulds are almost ready and I started to wonder if I need to post cure them? They are made from vinylester gelcoat, and polyester resin with fiberglass. If I need to post cure the moulds, how should I do it and do I need to leave the original fender inside the mould while doing it?

And the same applies to curing the parts. I will make the parts from carbon fiber and epoxy using infusion. How those should be cured? Parts inside the moulds or not? I will use this resin: https://composite24.co.uk/infusion-epoxy-resin-1-5kg

Also, how much resin I need? I am guessing that 1.5 kg/fender?


Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Wax release agents are usually known for their problem with elevated temperatures. The one in your link explicitly says that it's for room temperature use only. And the sun heats things up very unevenly. It could be that some spots got even higher than 55°C.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
okkim - 5 Years Ago
Steve Broad - 5 Years Ago
Warren (Staff) - 5 Years Ago
okkim - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
                     Of course, keep forgetting that we aren't talking prepreg here.
Steve Broad - 5 Years Ago
okkim - 5 Years Ago
Hanaldo - 5 Years Ago
okkim - 5 Years Ago
okkim - 5 Years Ago
oekmont - 5 Years Ago
okkim - 5 Years Ago
Hanaldo - 5 Years Ago
okkim - 5 Years Ago
okkim - 5 Years Ago
Hanaldo - 5 Years Ago
okkim - 5 Years Ago
Warren (Staff) - 5 Years Ago