Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
You wont be able to get in small quantities is the issue, have to buy it by the gallon. But if you've got a use for it, Trojan Fibreglass are probably your best bet. They have a couple of the Chemlease products that are very good. You don't NEED the sealer, but they do improve the product performance and I'd recommend it - price is hard to stomach.
CG Composites also had, but they have unfortunately just gone out of business. Places like Lavender and Ironbark have some of the more exotic products, but with a price tag to suit.
|