Okay so some will know I'm new to Vacuum Bagging and I want to,  I think I'm right in saying a Wet Layup. I'm planning to coat my Pre Waxed polished mould with Resin, lay some Carbon Fibre, stipple it with a brush, might lay some Glass Fibre on top of it, stipple it some more with resin and then I'll be ready for the next steps.

Is this the right things to do next, lay Peel Ply, then Perforated Release Film, then, Bleeder Ply and finally the bagging itself with a pressure of -5 to -8 HG until it cures, does this all sound right?
Edited 5 Years Ago by dilligaf76
Reply
dilligaf76
dilligaf76
Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)
Group: Forum Members
Posts: 49, Visits: 115
Well you still seem to know your stuff and the knowledge you do have is more than mine that’s for sure.
It’s interesting on how other people do theses things and great what I can take away from it. You’ve still been a big help to me and the only one so far on this post so thanks again Steve for all your input...

Edited 5 Years Ago by dilligaf76
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
dilligaf76 - 5 Years Ago
explorecomposites - 5 Years Ago
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
dilligaf76 - 5 Years Ago
Hanaldo - 5 Years Ago
dilligaf76 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search