Bagging tape definitely has an expiration date, it gets less tacky as it gets older. This is one reason I like the Cytec and Easy Composites tapes so much - they start off very tacky, which means that even as they get old they retain quite a good tack, and they are very pliable, which makes working them harder that much easier.
The AT200Y suffers badly with age. It is ok when it is brand new. But even by the time it is a year old, it has lost a lot of its tack. And because it is so firm, it is very taxing to work it and try to get it to stick properly.
|