Hi guys.

I ran into a bit of a problem today.

So i made e46 m3 hood. All good except for a little bulge (located in middle kevlar/cf "island on the right side o)n the top side (that i didnt notice untill todat when i took glued item from top mould) :/

After mild postcure (sun so max 50*C atm) it came out great so somwhere from that point to prior of bonding halves together this happend (inbetween i was only cutting vent holes).

Stack was as followed (top part) :
-245 2x2 cf
-600 2x2 cf
-200 cf/kevlar

All this time (apart from cutting & triming) paet was laying flat in mould to awoid any accidental damage in workshop. 

Halves arenow bonded and i can not seperate them again.

I was thinking of heating it gently locally with heat gun and then put so soft weight on and let it cool of (as atm TG is quite low...... plan was to let it full post cure bolted on the car and then sand it and get it clear coated). 

Any ideas how this happened and any alternative ways to solve it?

Thanks a lot

Edited 6 Years Ago by beliblisk
Reply
beliblisk
b
Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)Supreme Being (565 reputation)
Group: Forum Members
Posts: 53, Visits: 2.8K
Hi. 
I do always remove particles from the mould (just to avoid any unnecessary scratches) but that doesnt mean i got them all. This sounds possible and ill be extra careful from now on.

Any idea how to solve it besides my heat/weight "technique" ?

Thanks a lot


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
beliblisk - 6 Years Ago
MarkMK - 6 Years Ago
explorecomposites - 6 Years Ago
beliblisk - 6 Years Ago
explorecomposites - 6 Years Ago
beliblisk - 6 Years Ago
Hanaldo - 6 Years Ago
beliblisk - 6 Years Ago
Hanaldo - 6 Years Ago
beliblisk - 6 Years Ago
Steve Broad - 6 Years Ago
Hanaldo - 6 Years Ago
beliblisk - 6 Years Ago
Steve Broad - 6 Years Ago
beliblisk - 6 Years Ago
Hanaldo - 6 Years Ago
beliblisk - 6 Years Ago
Steve Broad - 6 Years Ago
Hanaldo - 6 Years Ago
Warren (Staff) - 6 Years Ago
Steve Broad - 6 Years Ago
beliblisk - 6 Years Ago
Steve Broad - 6 Years Ago
Hanaldo - 6 Years Ago
Steve Broad - 6 Years Ago
oekmont - 6 Years Ago
Steve Broad - 6 Years Ago
oekmont - 6 Years Ago
Steve Broad - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search