Polyester moulds and epoxy


Author
Message
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Hi guys, I was wondering if someone could clear something up for me as I've read conflicting information and now  I have a project where I need to know

Basically, I've been asked to make a part from epoxy using a mould which is being supplied.

The downside is the mould is made using polyester resin and some people say that I 100% won't be able to remove the part when finished, some say I need to use their special technique and combination of release agents and some say it'll be fine. Don't know if it'll make much difference, but I plan on using gc50 so hoping this will act as a decent barrier between the mould and epoxy

Some solid advice would be great. I've only ever had to use easy lease and wax and never had a problem making polyester parts in an epoxy mould.

I don't want to have to make a polyester buck, seal and make an epoxy mould as that cost will scare them away

Thanks in advance
Reply
mikew
mikew
Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)
Group: Forum Members
Posts: 56, Visits: 128
I'm interested in the answer to this as well. I'm using EL2 infusion resin and PVA as the release. It's tough to get the part out with PVA and I'd rather use easy lease and or wax but not confident without one of the guys here saying "yes that's ok"