FLD (14/12/2012)
You will run into issues if you bake the mold though Sad




Bringing up an old thread, but on this topic, I now need to make a structural part and it will be out in the sun quite a bit (assuming this British "summer" happens) so I need to post cure them to stop them softening.

As long as the polyester mould has been post cured before use to remove all styrene, then will it be ok? Not too worried about mould stability as they will pretty much be single use
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search