Hi, I’m looking to make a carbon fibre bonnet for my car. First time project, have done fibreglass panels before but not carbon fibre. I watched the video on YouTube on making a bonnet using the 200gsm cloth soric cloth and 200gsm cloth. Would I be able to use 200gsm first layer and a 600gsm second layer to make the bonnet? Would this have same or better strength? Secondly roughly speaking how much resin is required per sq metre? Thanks 

Replies
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
If using a core material like Soric, you are very likely going to get 'print through' on the surface, especially if you're looking to go quite light on fabric weight. This could possibly be overcome after production with flatting and clear coat, but it would add quite a bit of additional expense and labour time. Given the heat it would likely see afterwards, which could quickly cause some shrinkage of the resin and a less than flat appearance, it would be a good idea to post-cure it and then look to have it clear-coated after flatting down again. It would mean additional time and expense, but such a part can quickly begin to look less than perfect if left to the elements without any additional steps taken, given the application.  

Are you intending to mould and replicate the inner structure of the bonnet? If so, this should allow you to go a little lighter on the skin, as it will be supported much like the original. However, this calls for an additional mould to be made but might allow you to utilise fixings for the finished part more in line with the original fitment.

Large flat-ish panels on their own will be quite flexible if choosing to go with a 200g surface layer backed up by something like a 600/650g fabric. This would probably work okay with the inner structure bonded to the underside and a little additional localised reinforcement but it might be worth considering another layer of lighter fabric, at least, if you're thinking of replicating the bonnet as a single skin.






840csi
8
Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)
Group: Forum Members
Posts: 3, Visits: 39
MarkMK - 5/13/2020 6:30:53 AM
If using a core material like Soric, you are very likely going to get 'print through' on the surface, especially if you're looking to go quite light on fabric weight. This could possibly be overcome after production with flatting and clear coat, but it would add quite a bit of additional expense and labour time. Given the heat it would likely see afterwards, which could quickly cause some shrinkage of the resin and a less than flat appearance, it would be a good idea to post-cure it and then look to have it clear-coated after flatting down again. It would mean additional time and expense, but such a part can quickly begin to look less than perfect if left to the elements without any additional steps taken, given the application.  

Are you intending to mould and replicate the inner structure of the bonnet? If so, this should allow you to go a little lighter on the skin, as it will be supported much like the original. However, this calls for an additional mould to be made but might allow you to utilise fixings for the finished part more in line with the original fitment.

Large flat-ish panels on their own will be quite flexible if choosing to go with a 200g surface layer backed up by something like a 600/650g fabric. This would probably work okay with the inner structure bonded to the underside and a little additional localised reinforcement but it might be worth considering another layer of lighter fabric, at least, if you're thinking of replicating the bonnet as a single skin.






Hi guys, thanks for the advise you have both given. The bonnet I’m wanting to make is for a Range Rover (Large😞) I have made my own body kit for the car and hence had to modify and make a new bonnet using fibreglass (wet laid). This came out perfect fits and looks good only problem is that it is very heavy being fibreglass. For this reason I’m wanting to take the next step and try carbon fibre to reduce weight. I have moulds for the bonnet and the under structure and will be making both parts and bonding together. I’m also looking to purchase the infusion and vacuum bagging kits here, so I can infuse it rather than wet lay. What would be best layout for the bonnet for strength and weight?  eg: several layers of carbon only or carbon with soric layer using the infusion method to make parts. Thanks 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
840csi - 5 Years Ago
Steve Broad - 5 Years Ago
MarkMK - 5 Years Ago
840csi - 5 Years Ago
oekmont - 5 Years Ago
840csi - 5 Years Ago
MarkMK - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search