Hi I’m struggling to work out how to skin a dashboard bezel or similar round item . I need to know how to get it around the item and fold inside to cover the bezel. Do I cut a strip or lay a piece over and cut a hole in the middle? I’m stuck please help
Edited 5 Years Ago by Leegsy
Replies
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Leegsy, I'm trying to get my head around what you've got without the picture too. It's tough!

Maybe we should try to get to the bottom of the picture uploading problem, then we can try to give you some good advice on your conundrum! I'll try uploading an image in a second post to this message to check the system. Could you also let me know what you're trying to upload (file format, image size) and what device/platform/OS/browser you're using?

Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Leegsy
L
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 3, Visits: 8
Hi yeah using iPhone to upload from saved images , don’t know if that’s the problem but have tried and tried , once I get some idea how to do this it pretty much covers me for all pieces I want to do email maybe?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Leegsy - 5/12/2020 9:07:32 AM
Hi yeah using iPhone to upload from saved images , don’t know if that’s the problem but have tried and tried , once I get some idea how to do this it pretty much covers me for all pieces I want to do email maybe?

Hi Leegsy, thanks for that. Yes, perhaps it's an iPhone issue. I'll run this past the forum technical chap and see if we can get to the bottom of it. In the meantime, yes, please just email images to technical@easycomposites.co.uk. I could even post them on here so we can discuss.
Thanks, Matt


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Leegsy - 5 Years Ago
Hanaldo - 5 Years Ago
Leegsy - 5 Years Ago
Matt (Staff) - 5 Years Ago
Leegsy - 5 Years Ago
Matt (Staff) - 5 Years Ago
Warren (Staff) - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search