On infusion resin, how long time is it to cure??
And if I lower the temperature during the infusion time, will it be longer time and ok, and then raise the temperature when infusion are clear??
Does the epoxi infusion have minimum temperature to get infusion or are 0 c the lowest and still good for increasing the heat after it have bin pulled thru mold??

/Nicklas

Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
The exact temperature doesn't really makes a difference how far you can get with your infusion, as long as it is around room temperature (wich it should be). If it is a little colder, the pot life is longer, but the resin flows equally much slower. Most infusion resin systems have 2-3 differnt hardener options, from slow to fast curing.