Hello,
what is the difference between Resin Infusion Starter Kit, Vacuum Bagging Starter Kit  & Regular Prepreg Carbon Fibre Starter Kit?
I am using only wet lay up right now and was thinking about upgrading the quality of the part I was making.

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The kits are for three completely different processes.

Vacuum bagging
Resin Infusion
Pre-preg

Vacuum bagging is similar to what you do now, you just stick the finished part in a vacuum bag, pull about 20% vacuum and let it cure.

Resin Infusion and pre-preg are a bit more complicated and I would recommend you watch the videos on each process here:  Online Composites Learning Area

All three processes (and wet lay) can have good cosmetic results, although you will find infusion and pre-preg are more about proper process control rather than wet lay which needs a fair bit of skill and experience to get good results.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant