By benji - 4/27/2020 5:16:11 PM
Hello, what is the difference between Resin Infusion Starter Kit, Vacuum Bagging Starter Kit & Regular Prepreg Carbon Fibre Starter Kit? I am using only wet lay up right now and was thinking about upgrading the quality of the part I was making.
|
By Warren (Staff) - 4/28/2020 1:55:18 PM
The kits are for three completely different processes.
Vacuum bagging Resin Infusion Pre-preg
Vacuum bagging is similar to what you do now, you just stick the finished part in a vacuum bag, pull about 20% vacuum and let it cure.
Resin Infusion and pre-preg are a bit more complicated and I would recommend you watch the videos on each process here: Online Composites Learning Area
All three processes (and wet lay) can have good cosmetic results, although you will find infusion and pre-preg are more about proper process control rather than wet lay which needs a fair bit of skill and experience to get good results.
|
|