So a few years back I made up several mould tools using Uni-Mould and the intention to use the Easy-Preg and Vari-Preg products as at the time it was the standard choice for Out of Autoclave.
Now that a few years have passed and things have moved to the new X-Preg System which I notice is not compatible with the Uni-Mould system, Do I now have a load of mould tools that I cannot use or is there a way for me to still use these moulds with the X-Preg system?

 I'll be a little annoyed if all the money invested in making these moulds goes to waste. Obviously now any future moulds I make will use X-Preg Tooling


Shaneer22
Shaneer22
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
RyanParle - 4/27/2020 1:34:59 PM
So a few years back I made up several mould tools using Uni-Mould and the intention to use the Easy-Preg and Vari-Preg products as at the time it was the standard choice for Out of Autoclave.
Now that a few years have passed and things have moved to the new X-Preg System which I notice is not compatible with the Uni-Mould system, Do I now have a load of mould tools that I cannot use or is there a way for me to still use these moulds with the X-Preg system?

 I'll be a little annoyed if all the money invested in making these moulds goes to waste. Obviously now any future moulds I make will use X-Preg Tooling


I would post cure to 90 and use board sealer.

Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The moulds will still work just fine. Easy Composites official stand point on it is that vinyl tooling causes pinholing with the X-Preg system. I've done extensive testing with this, and I've found I get exactly the same results with vinyl tooling as I do with epoxy tooling, but the vinyl tooling seems to start to suffer a little bit earlier, ill only get 10 or 15 pulls before release becomes a bit harder (still ok, but no longer falling out of the mould) and little bits of gelcoat start to come off. With regards to the X-Preg component quality - exactly the same with epoxy and vinyl tooling.

I have found a much longer post-cure on the tooling before putting it into service helps. I'll do a regular post-cure cycle, but then do an extended soak at 90° for minimum 24 hours.