Hello, at the moment I prefer to brush gelcoats or pattern coats as I don't have the proper equipment to spray.
Despite the quality of the brush and some thinning, I always end up with brush strokes so a lot of high and low spots.
What is your recommended tool to flatten out the brush strokes?
Besides manual sanding, I am looking into orbital and roto-orbital sanders but not sure what works best or if exist better tools for the job.
Any feedback would be greatly appreciated!
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Random orbital.
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 4/26/2020 1:22:44 PM
Random orbital.

Thanks!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search