Make sense from what perspective? Cost? Weight saving? Ease of building? Strength? Could be a yes or a no depending on what your priorities are.
Strength wise, mechanically fastening to composites is never ideal, unless you have designed for it. Simply drilling a hole and putting a bolt and nut through a fibreglass laminate will put stress on the laminate and be a weak point over time. So for me, bonding is better - whether that means bonding the U-section or bonding in a fastener to the fibreglass to facilitate bolting. You could simply bond a SS U-section to the fibreglass using an appropriate adhesive, it wouldn't have to be fibreglass.
|