Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
Thank you, I truly and kindly appreciate it! It all makes sense to me now. 

I also understand that I am to weigh the amount of Carbon Fibre I chose and from that I can define how much resin to use. How does that weighing system work based on the weight of the Carbon? 
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
For simple wet lay that works fine.  You don't need to physically weigh it out if that's a bit awkward, just calculate it from the nominal weight of the cloth and surface area used.  eg a 200gsm cloth, 2sqm and 4 layers would need 1.6kg of resin plus a little extra for waste etc. 

If you do infusion, you can take into account resin uptake of the peel ply, mesh and bit for spiral and hoses.  You can also reduce the resin ratio to 60:40 fibre:resin as it is more efficient.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited 6 Years Ago by Warren (Staff)
Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
Thank you, much appreciated!

As seen on the photo below I have been getting this white sort of finish. the reflection of the light is pretty clear. However, that the scratches and the "White finish" is ruining the part. What could this be? The resin, the finish of the plug?

Once again, any suggestions on how to avoid this and get a great finish would be appreciated it. 




Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Its hard to tell in photos but it could be slight marring on the mould surface, a slight witness mark from the release agent?  How was the release? did it come off easily?  Sometimes on thin sheets, if the release is a bit tougher than usual, as you peel the sheet off you can get the beginning of stress fractures or cracks where it flexes a little too much and that can look like that before it becomes proper visual cracks if flexed even further. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
On that attempt, I used just Wax Mold Release and not a chemical release agent. I will now try with a chemical one on a polished glass surface as we discussed earlier and can definitely let you know what I get!

Thank you once again!

Rafael

Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
I am back with another question.

What is the best way to properly apply Duratec Surface Primer (707-002)? As in sanding, cure time and so on?  

Thanks in advance

Rafael
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I would follow the manufacturers recommendations. Its not a product I have used personally.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
I hope all is well with everyone!

I finally managed to produce a usable Mold. Though, now that I reached this stage, what is the next best recommended move to ready the mold? Would I need to wet sand it, polish it, then add mold sealer and so on? (The mold was produced using Black Tooling Gelcoat)

Any suggestions would be kindly appreciated. 

Raf
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If the finish is not already high gloss and smooth, then sand it smooth and then polish it to a high gloss then you should have a tool ready to go.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
Thanks Warren!