Raf, from Canada


Author
Message
Rafael Piccoli
R
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 19, Visits: 84
Glad to be here!
I have started working with composites just recently and looking to add it to my Industrial Design Portfolio.

I have one question to start off with. What is the best material to use as a plug to laminate a simple carbon fibre plate through vacuum infusion? I have tried acrylic and aluminum. However, it never comes out with a clear and clean look.

I would appreciate any suggestions.

Thank you



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
rafapiccoli - 6 Years Ago
MarkMK - 6 Years Ago
Warren (Staff) - 6 Years Ago
rafapiccoli - 6 Years Ago
Hanaldo - 6 Years Ago
rafapiccoli - 6 Years Ago
SleepingAwake - 6 Years Ago
rafapiccoli - 6 Years Ago
SleepingAwake - 6 Years Ago
MarkMK - 6 Years Ago
rafapiccoli - 6 Years Ago
Warren (Staff) - 6 Years Ago
rafapiccoli - 6 Years Ago
Warren (Staff) - 6 Years Ago
rafapiccoli - 6 Years Ago
rafapiccoli - 6 Years Ago
Warren (Staff) - 6 Years Ago
rafapiccoli - 6 Years Ago
Warren (Staff) - 6 Years Ago
             Thanks Warren!
rafapiccoli - 6 Years Ago
rafapiccoli - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search