Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
If the finish is not already high gloss and smooth, then sand it smooth and then polish it to a high gloss then you should have a tool ready to go.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|