	Group: Forum Members 	        
    Posts: 680, 
    Visits: 1.9K 
    
 
          
		     | 
				                       
                 
                
                    
			            If you ran the spiral all the way along the top (longest) edge I don't understand how resin could possibly not 'get there' - it would be pretty much starting there. Can you upload a photo of what happened?                
			            
  				
			            Matt Statham Easy Composites / Carbon Mods - Technical Sales                     
                     
                                            
                         
                    
                  
             |