            I would like some advice from you more experienced folk, I am infusing an odd shaped panel, se image, and would like to know the best place to put the vac and resin lines? The sheet will be a decorative piece in 195g c/f. Thanks.
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By fgayford - 11/25/2012 7:31:35 PM				
            
                      
            I have done it many times and it works well. The only thing I didn't like is that the feed line where it contacted the center of the part left a slight impression. Being a perfect cosmetic carbon fiber look was what I was after I now infuse across the part left to right.
  Fred  
           
		 | 			
		 
	
	
						
		 	
		
	 |